Molding test environment and standards:
|
|
①Temperature: 23±2℃
|
|
②Relative humidity: 50%RH±5%RH
|
|
③Test spline standard: ASTM
|
|
④ Post-curing conditions: Put the test strip in water and post-cure the front and back sides under 200mw/cm² of 405-band ultraviolet rays 1 minute.
|
|
Technical parameters after molding:
|
|
Maximum force (KGF)
|
108.7±10%
|
Tensile strength (MPa)
|
25.62±10%
|
Deformation at the point of maximum force (mm)
|
9.99±10%
|
Elongation at yield point (%)
|
5.50±10%
|
Elongation at break (%)
|
17.65±10%
|
Maximum bending strength (MPa)
|
25.48±10%
|
Flexural modulus of elasticity (MPa)
|
693.51±10%
|
Shore hardness (D)
|
80~85
|
Impact strength (j/m)
|
118.46±10%
|
Tensile modulus (MPa)
|
320.80±10%
|